Specific Process Knowledge/Characterization/Sample imaging
Appearance
The list of instruments for sample imaging available at Danchip includes a number of optical microscopes , three scanning electron microscopes (SEM's) and an atomic force microscope (AFM).
| Optical microscopes | SEM | AFM | Profiler | |
|---|---|---|---|---|
| Magnification range | ||||
| Depth of focus |