Specific Process Knowledge/Thin film deposition/Deposition of Tungsten
Feedback to this page: click here
Tungsten (W) can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | |
---|---|
Batch size |
|
Pre-clean | RF Ar clean |
Layer thickness | 10Å to 5000Å* |
Deposition rate | 2Å/s to 15Å/s |
Allowed materials |
|
Comments |
* For thicknesses above 200 nm permission is required