Specific Process Knowledge/Thin film deposition/Deposition of Molybdenum
Feedback to this page: click here
Molybdenum deposition
Molybdenum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. In PVD co-sputter/evaporation only VERY thin layers of Mo can be deposited.
E-beam evaporation (Alcatel) | E-beam evaporation (PVD co-sputter/evaporation) | |
---|---|---|
Batch size |
|
|
Pre-clean | RF Ar clean | RF Ar clean |
Layer thickness | 10Å to 0.5 µm* | 10Å to 500 Å |
Deposition rate | 2Å/s to 15Å/s | About 1 Å/s |
Allowed materials |
|
|
Comment | Only very thin layers (up to 100nm). |
* For thicknesses above 200 nm permission from ThinFilm group (thinfilm@danchip.dtu.dk) is required.