Specific Process Knowledge/Thermal Process/Annealing
Appearance
Feedback to this page: click here
Annealing
At Danchip we have three furnaces and an RTP (Rapid thermal annealing) that can be used annealing: C1, C3, Noble furnace and Jipelec RTP. Annealing normally takes place in an N2 atmosphere. PECVD PBSG glass is annealed in a wet atmosphere which will also oxidize the silicon substrate.
The recipes for oxidation are made so that a 20 minutes N2 annealing step is included after the oxiation step.
Comparison of the annealing furnaces
| General description | Annealing of 6" wafers. Annealing of wafers from the LPCVD furnaces and PECVD1. | Annealing of wafers from EVG-NIL, PECVD3 and wafers with aluminum. | Annealing of almost materials on silicon wafer. | Rapid thermal annealing |
|---|---|---|---|---|
| Annealing gas |
|
|
|
|
| Process temperature |
|
|
|
|
| Substrate and Batch size |
|
|
|
|
| Allowed materials |
|
|
|
|