Specific Process Knowledge/Thermal Process/Furnace APOX
Appearance
Feedback to this page: click here
Apox furnace (D1)
The APOX furnace (D1) is a Tempress horizontal furnace for oxidation silicon wafers. This furnace is dedicated production of apox wafers which is a very thick thermal oxide grown at 1150 oC. Running a batch of apox wafers (oxide>5µm) can take several weeks.
This furnace is positioned in III-V cleanroom. The furnaces are the cleanest process chambers in the cleanroom. Only new wafers from the box enters this furnace.
Process knowledge
- Oxidation: look at the Oxidation page
| Purpose | Oxidation and annealing | Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|