Molybdenum deposition
Molybdenum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. In PVD co-sputter/evaporation only VERY thin layers of Mo can be deposited.
| E-beam evaporation (Alcatel) | E-beam evaporation (PVD co-sputter/evaporation) | |
|---|---|---|
| Batch size |
|
|
| Pre-clean | RF Ar clean | RF Ar clean |
| Layer thickness | 10Å to 0.5 µm | 10Å to 500 Å |
| Deposition rate | 2Å/s to 15Å/s | About 1 Å/s |
| Comment | Only very thin layers (up to 100nm). |