Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBE magnetic stack etch
Results of Design of Experiments optimization of magnetic stack etching
Process parameters for the acceptance test
Parameter | Ti etch acceptance |
---|---|
Neutalizer current [mA] | 450 |
RF Power [W] | 800 |
Beam current [mA] | 400 |
Beam voltage [V] | 500 |
Beam accelerator voltage | 500 |
Ar flow to neutralizer [sccm] | 5.0 |
Ar flow to beam [sccm] | 10.0 |
Rotation speed [rpm] | 20 |
Stage angle [degrees] | 5 |
Helium backside cooling [Torr] | 37.5 |