Plasma cleaner: 2 & 3

Plasma Cleaner: 2 is located in PolyFabLab, and Plasma Cleaner: 3 is located in the PDMS lab in building 347.
Plasma Cleaner: 2 is located in PolyFabLab, and Plasma Cleaner: 3 is located in the PDMS lab in building 347.

Plasma cleaner 2 (located in PolyFaLab) and Plasma cleaner 3 (located in PDMS lab) are Diener Atto (PC control, 13.56 MHz RF) systems installed in 2026. The primary purpose of the plasma cleaners is surface cleaning and activation of polymer films.