Palladium deposition
Palladium can be deposited by e-beam evaporation or DC sputtering at DTU Nanolab.
Sputtering of Palladium
Palladium may be sputter deposited in the sputter-system (Lesker). See process results here:
Equipment comparison
In the chart below you can compare the different deposition equipment:
| E-beam evaporation (Temescal and E-beam evaporator (10-pockets)) | Sputter deposition (Sputter-System (Lesker)) | Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | ||
|---|---|---|---|---|
| General description | E-beam deposition of Pd | Sputter deposition of Pd | Sputter deposition of Pd | |
| Pre-clean | Ar ion source (only in E-beam Evaporator Temescal) | none | RF Ar clean | |
| Layer thickness | 10 Å - 600 nm* | 10 Å - 600 nm* | 10 Å - ? discuss with staff | |
| Deposition rate | 0.5 Å/s to 10Å/s | Up to 4.3 Å/s | Discuss with staff | |
| Batch size |
|
|
| |
| Allowed materials |
|
|
Almost any that does not degas at your intended substrate temperature. See cross contamination sheets for PC1 and PC3 | |
| Comment |
* If depositing more than 600 nm, please write to metal@nanolab.dtu.dk well in advance to ensure that enough material is present.