Molybdenum deposition
Molybdenum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Temescal) | Sputter deposition (Lesker) | Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | |
|---|---|---|---|
| General description | E-beam deposition of Mo
(line-of-sight deposition) |
Sputter deposition of Mo
(not line-of-sight) |
Sputter deposition of Mo
(not line-of-sight) |
| Pre-clean | Ar ion source | RF Ar clean | RF Ar clean |
| Layer thickness | 10Å to 0.2 µm* | 10Å to 500 Å | 10Å to ? discuss with staff |
| Deposition rate | 1Å/s to 10Å/s | Depends on process parameters, roughly about 1 Å/s | Not known yet, probably similar to 'old' Lesker sputter system |
| Batch size |
|
|
|
| Allowed materials |
|
|
Almost any as long as it does not outgas. |
| Comment | Sputter target size 2". | Sputter target size 3-4" (usually 3"). So far (June 2025) Mo has been deposited in PC1. See process log for details. |
* Depending on the amount of heating during Mo deposition, which we will discover during process development.