Jump to content

Specific Process Knowledge/Characterization/XPS/Processing/Basics/3fitting

From LabAdviser
Revision as of 10:36, 4 September 2025 by Jmli (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Feedback to this page: click here

Unless otherwise stated, the content of this page was created by the dry etch group at DTU Nanolab

Fitting the oxygen O1s core level

There is a few choices to make on the fitting of the O1s level. The level is an s-orbital and thus gives rise to a peak that is symmetric so any non-symmetric appearance must be caused several states of oxygen. The question is then to which states of oxygen they should be attributed. Below are shown the spectra of levels 0 (surface), 11 and 20.

Level 0 Level 11 Level 20

We can establish that

  • The main peak remains at fixed binding energy, and
  • There is a shoulder at higher binding energy