Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
15/12-2014 4" Wafer with AZ resist Travka50 pattern Si / 50 % Pegasus/jmli 20 minute TDESC clean nanolab/jml/showerhead/prD/New Process D, 75 cycles or 5:00 minutes S004743 New showerhead