Specific Process Knowledge/Thin film deposition/Deposition of Nickel
Feedback to this page: click here
Nickel deposition
Nickel can be deposited by e-beam evaporation, sputtering or electroplating. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | Sputter deposition (Lesker) | Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | Electroplating (Electroplating-Ni) | |
|---|---|---|---|---|---|
| General description | E-beam deposition of Nickel | E-beam deposition of Nickel | Sputter deposition of Nickel | Sputter deposition of Nickel | Electroplating of Nickel |
| Pre-clean | Ar ion bombardment | RF Ar clean | RF Ar clean | None | |
| Layer thickness | 10 Å to 1 µm * | 10 Å to 1 µm * | 10 Å to 5000 Å ** | 10 Å to 5000 Å ** | ~ 20 µm to ~ 1000 µm |
| Deposition rate | 2-10 Å/s | 10-15 Å/s | Depends on process parameters, about 1 Å/s | Depends on process parameters, at least ~ 4 Å/s, see conditions here | ~ 10-250 Å/s |
| Batch size |
|
|
|
|
|
| Allowed materials |
|
|
|
|
Base materials:
Seed metals:
|
| Comment |
|
|
|
* To deposit a cumulative thickness above 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine
** To deposit a cumulative thickness above 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine
Quality control of e-beam evaporated Ni films
| Quality control (QC) for Wordentec | ||||||||||||||||
Thickness is measured in 5 points with a stylus profiler. |
| Quality control (QC) for the Temescal | ||||||||||||||||||
Thickness is measured in 5 points with a stylus profiler. |