Specific Process Knowledge/Thin film deposition/Deposition of Platinum
Feedback to this page: click here
Platinum deposition
Platinum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | Sputter deposition (Lesker) | ||
---|---|---|---|---|
General description | E-beam deposition of Pt | E-beam deposition of Pt | Sputter deposition of Pt | |
Pre-clean | Ar ion source | RF Ar clean | RF Ar clean | |
Layer thickness | 10Å - 1µm* | 10Å to 5000Å* | 10Å to 5000Å | |
Deposition rate | 0.5Å/s to 10Å/s | 10Å/s to 15Å/s | ? Å/s to ? Å/s | |
Batch size |
|
|
| |
Allowed materials |
|
|
| |
Comment |
* If depositing a total of more than 600 nm, please write to metal@danchip.dtu.dk well in advance to ensure that enough material is present.