Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
28/2-2014 4" travka50 wafer 1.5 µm AZ Si / 50 % Pegasus/jmli 1 minute TDESC clean + MU runs jml/isotropic/isoslow7 1:00 minutes S003900 Bottom fine!!