Specific Process Knowledge/Thin film deposition/Deposition of Titanium
Titanium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | E-beam evaporation (Wordentec) | Sputter deposition (Wordentec) | |
---|---|---|---|
Batch size |
|
|
|
Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean |
Layer thickness | 10Å to 1µm | 10Å to 1 µm | . |
Deposition rate | 2Å/s to 15Å/s | 10Å/s to 15Å/s | Depending on process parameters, see here. |