Specific Process Knowledge/Thin film deposition/Deposition of Titanium Nitride

From LabAdviser

Feedback to this page: click here


Deposition of Titanium nitride

Thin films of titanium nitride can be deposited by ALD and sputering methods.

Information about the ALD process can be found here.

Information about the sputtering process can be found here.

Comparison between sputtering and ALD methods for deposition of Titanium Nitride.

ALD2 Sputter System Lesker
Generel description
  • Atomic Layer Deposition
  • Sputtering
Stoichiometry
  • TiN
  • TiN (can be tuned)
Film Thickness
  • 0nm - 50nm
  • 0nm - 200nm
Deposition rate
  • 0.0173 nm/cycle on a flat sample
  • 0.0232 nm/cycle on a high aspect ratio structures
  • up to 0.0625 nm/s on a flat sample
Step coverage
  • Very good
  • Not investigated
Process Temperature
  • 450oC
  • 400oC
Substrate size
  • Several small samples
  • 1-5 50 mm wafers
  • 1-5 100 mm wafers
  • 1-5 150 mm wafer
  • Several small samples
  • 100 mm wafer
  • 150 mm wafer
Allowed materials
  • Silicon
  • Silicon oxide, silicon nitride
  • Quartz/fused silica
  • Al, Al2O3
  • Ti, TiO2
  • Other metals (use dedicated carrier wafer)
  • III-V materials (use dedicated carrier wafer)
  • Polymers (depending on the melting point/deposition temperature, use carrier wafer)
  • Silicon
  • Silicon oxide, silicon nitride
  • Quartz/fused silica
  • Metals
  • III-V materials (use dedicated carrier wafer)
  • Almost anything that is not toxic.