Deposition of Nickel Iron alloy
Nickel Iron alloy, e.g., Invar, has been sputter deposited in the Sputter-system (Lesker) here at Nanolab.
You will find detailed results of varying the process parameters when sputtering Ni-Fe in the Lesker sputter system here.