Specific Process Knowledge/Thin film deposition/Deposition of Titanium
Titanium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | E-beam evaporation (Leybold) | E-beam evaporation (Wordentec) | Sputter deposition (Wordentec) | ||
---|---|---|---|---|---|
Batch size |
|
|
|
| |
Pre-clean | RF Ar clean | Ar ion bombartment | RF Ar clean | RF Ar clean | |
Layer thickness | 10Å to 1µm | 10Å to 0.5µm | 10Å to 1 µm | . | |
Deposition rate | 2Å/s to 15Å/s | 1Å/s to 5Å/s | 10Å/s to 15Å/s | . | Dependent on process parameters |