The Die-bonder Cammax EDB-80 is placed in the Packlab in building 347, 1st floor.
Heating Chuck on the Die-bonder

Die bonder (eutectic metal soldering)

The Cammax EDB80 Die bonder is for placing and soldering dies onto a package or substrate.

The bonder has a graphite heater element enabling fast heating to the melting point of the solder. To prevent oxidation of the solder and bonding surfaces it is possible to have a gas flow of formier gas (4-10% H2 in N2) over the sample. The machine also has a pick-up tool enabling accurate placement of the sample onto a carrier.

The user manuals, user APVs, technical information and contact information can be found in LabManager:

Die Bonder in LabManager

Process information









Equipment performance and process related parameters

Equipment Die bonder Flip-chip bonder
Purpose
  • Fine placement of dies
  • Eutectic metal soldering
  • Fine placement of dies
  • Glue attachment
Performance
  • Low thermal resistance
  • Always conducting
  • Medium or High thermal resistance
  • Possibility of both conducting and isolating adhesives
  • If an epoxy based adhesive is used the user is required to have the epoxy course.
Substrates Allowed materials
  • Should be able to withstand the soldering temperature
  • Typical materials are: Alumina (Al2O3), AluminumNitride (AlN)
  • Any that is compatible with the glue and temperature used