Specific Process Knowledge/Thin film deposition/Deposition of Palladium
Feedback to this page: click here
Palladium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment:
E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | |
---|---|---|
General description | E-beam deposition of Pd | E-beam deposition of Pd |
Pre-clean | Ar ion source | RF Ar clean |
Layer thickness | 10 Å - 1 µm* | 10 Å to 200 nm |
Deposition rate | 0.5 Å/s to 10Å/s | 2 Å/s to 10Å/s |
Batch size |
|
|
Allowed materials |
|
|
Comment |
* If depositing more than 600 nm, please write to metal@danchip.dtu.dk well in advance to ensure that enough material is present.