ZnO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment.
| Sputtering deposition (Lesker) | Atomic layer deposition (ALD Picosun R200) | |
|---|---|---|
| General description | Sputter deposition of ZnO | Atomic layer deposition of ZnO |
| Pre-clean | RF Ar clean | |
| Layer thickness | 10Å to 5000Å* | 0 to 1000 Å |
| Deposition rate | Depending on process parameters. | Depending on temperature |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment |
|
* For thicknesses above 200 nm permission is required.