Recipe

Recipe name SiH4 flow [sccm] N2O flow [sccm] N2 flow [sccm] B2H6 flow [sccm] Pressure [mTorr] Power [W] Description
1PBSG 17 1600 0 135 500 800LF BPSG glass for drive in boron in Silcion