Jump to content

Specific Process Knowledge/Thermal Process/Furnace: Multipurpose annealing/Acceptance test

From LabAdviser

THIS PAGE IS UNDER CONSTRUCTION

Recipe: "vr_dryOx_1000C_120min_150_5Wafer_D1_mit_Inliner_oPurgering.ATV"

Oxidation time: 80 min Oxidation temperature: 1050 oC O2 flow: 1 slm

The oxidation has been done with 150 mm wafer, and with 30 wafers in the furnace.

Wafer 4 (towards the door), wafer 16 and wafer 28 (towards the service area) were measured.


The acceptance for the Multipurpose Anneal furnace was performed in November 2014 by ATV Technologie.