Specific Process Knowledge/Thin film deposition/Deposition of Copper
Feedback to this page: click here
Deposition of Cu
Copper can be deposited by e-beam evaporation, sputtering or electroplating. In the chart below you can compare the different deposition equipments.
E-beam evaporation (Alcatel) | Sputter deposition (PVD co-sputter/evaporation) | Sputter deposition (Lesker) | Electroplating (Electroplating-Cu) | |
---|---|---|---|---|
General description | E-beam deposition of Cu | Sputter deposition of Cu | Sputter deposition of Cu | Electroplating of Cu |
Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean | None |
Layer thickness | 10Å to 0.5µm* | 10Å to 1µm* | 10Å to 1µm* | thickness window undefined yet |
Deposition rate | 2Å/s to 15Å/s |
Depending on process parameters |
~1Å/s | |
Batch size |
|
|
|
|
Allowed materials |
|
|
almost any | Base Materials:
Seed metals:
|
Comment | Sample must be compatible with plating bath. Seed metal layer required to run electroplating process. |
* To deposit layers thicker then 200 nm permission is required (contact Thin film group)
Studies of Cu deposition processes
Roughness of Cu layers - Roughness of Cu layers deposited with Alcatel