Specific Process Knowledge/Etch/KOH Etch

From LabAdviser

KOH etch - Anisotropic silicon etch

KOH etch for 4" wafers: positioned in cleanroom 3

KOH belongs to the family of anisotropic Si-etchants based on aqueous alkaline solutions. The anisotropy stems from the different etch rates in different crystal directions. The {111}-planes are almost inert whereas the etch rates of e.g. {100}- and {110}-planes are several orders of magnitude faster.

At Danchip we use as a standard a 28 wt% KOH.

Wet etching of aluminium is done with two different solutions:

  1. H2O:H3PO4 1:2 at 50 oC
  2. Pre-mixed etch solution: PES 77-19-04 at 20 oC

Both solutions are used in the Aluminium etch bath shown to the right. I must be written on which one is in. Solution no. 1 is the most used solution for etchning oure aluminium. Solution no. 2 is primarily for etching aluminium mixed with a small percentage of silicon.


Comparing the two solutions

Aluminium Etch 1 Aluminium Etch 2
General description

Etch of pure aluminium

Etch of aluminium + 1.5% Si

Chemical solution H2O:H3PO4 1:2 PES 77-19-04
Process temperature 50 oC 20 oC
Possible masking materials:

Photoresist (1.5 µm AZ5214E)

Photoresist (1.5 µm AZ5214E)

Etch rate

~100 nm/min (Pure Al)

~60(??) nm/min

Batch size

1-25 wafers at a time

1-25 wafer at a time

Size of substrate

4" wafers

4" wafers

Allowed materials
  • Aluminium
  • Silicon
  • Silicon Oxide
  • Silicon Nitride
  • Silicon Oxynitride
  • Photoresist
  • E-beam resist
  • Aluminium
  • Silicon
  • Silicon Oxide
  • Silicon Nitride
  • Silicon Oxynitride
  • Photoresist
  • E-beam resist