Polymer injection molding
The injection molder at Danchip is an Engel Victory Tech 80/45. It is a hydraulic machine capable of up to 450 kN of clamping force.
The user manual, user APV, technical information and contact information can be found in LabManager:
Process information
There are no standard processes on the injection molder, since the type of process chosen and process parameters will depend on which polymer that will be used and what type of pattern that is to be replicated during the molding process. At Danchip the following polymers are used routinely:
Topas 5013L-10
Topas 8007S-04
PP
PMMA
Topas polymers are supplied by Danchip. All other polymers are purchased by the users themselves. All polymers must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the request form found in LabManager here.
| Parameter | Value | |
|---|---|---|
| Processing temperatures | Mold |
Up to 160*C |
| Barrel |
Absolute max: 350*C | |
| Processing temperatures | Temperature |
Up to 160*C |
| Barrel |
Absolute max: 350*C | |
| Molding parameters | Injection speed |
Up to 53 cm3/s |
| Injection pressure |
Up to 2200 bar | |
| Switch-over point |
Time, pressure, volumen or external signal | |