This is a micrometer-screw.

The Leo SEM has its own dedicated room: Cleanroom 9

It measures with an accurracy within a few µm. Measure the wafer in the box next to the meter.If ok other wafers can be measured. There is a calibration by the DEKTAK. It is calibrated at about 750µ