- 11:15, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check page 3.pdf (Unifromity of CNTS from BM)
- 09:47, 9 November 2012 Kn talk contribs uploaded File:CNTS uniformity check.pdf (Carbon nanotubes from black magic. Uniformity across a wafer checked, and summarized in this file. )
- 16:45, 7 November 2012 Kn talk contribs uploaded File:CNTS uniformity check.pptx (Presenstation of a short study that was made to check the uniformity of CNTs grown in the Black magic system.)
- 12:17, 7 November 2012 Kn talk contribs uploaded File:W5 center.JPG (CNTs, wafer 5. Recipe "PECVD NH3.txt" 5 min growth.)
- 11:07, 7 November 2012 Kn talk contribs uploaded a new version of File:W6 center oposit.tif (CNTs wafer 6, recipe "PECVD NH3. txt")
- 11:06, 7 November 2012 Kn talk contribs uploaded File:W6 center oposit.tif (CNTs wafer 6, recipe "PECVD NH3.txt")
- 11:52, 6 November 2012 Kn talk contribs uploaded File:W3 center CNTs.JPG (Black Magic CNTs. recipe "PECVD NH3.txt" 10 min growth.)
- 11:48, 6 November 2012 Kn talk contribs uploaded File:W3 center CNTs.tif (Black Magic CNTs. recipe "PECVD NH3.txt" 10 min growth.)
- 13:36, 8 October 2012 Kn talk contribs uploaded File:Dektak 8 new position.JPG
- 15:48, 5 October 2012 Kn talk contribs uploaded File:Dektak XTA new.JPG (Dektak XTA)
- 13:21, 20 September 2012 Kn talk contribs uploaded File:Wafer plate.JPG (Wafer plate for PVD co-sputter/evaporation.)
- 14:54, 18 June 2012 Kn talk contribs uploaded File:III-V profiler.JPG (III-V profiler)
- 15:58, 15 June 2012 Kn talk contribs uploaded File:Physimeca.jpg (Physimeca)
- 15:41, 15 June 2012 Kn talk contribs uploaded File:P1040003.JPG (Chamber III-V dielectric evaporator)
- 15:40, 15 June 2012 Kn talk contribs uploaded File:IMG 3070.jpg (Picture of rack to the III-V Dielectric evap)
- 16:02, 5 January 2012 Kn talk contribs uploaded File:MWNT Kapar Haume.JPG (Example MWNT from Black Magic)
- 09:51, 4 January 2012 Kn talk contribs uploaded File:BM chamber.JPG (Open Black magic chamber)
- 10:29, 3 January 2012 Kn talk contribs uploaded File:Black magic PECVD.JPG
- 15:29, 25 October 2011 Kn talk contribs uploaded File:Schematic XPS.JPG
- 15:25, 25 October 2011 Kn talk contribs uploaded File:XPS electron levels.pdf
- 15:23, 25 October 2011 Kn talk contribs uploaded File:XPS electron levels.pptx
- 09:27, 24 October 2011 Kn talk contribs uploaded File:Si2p.JPG (XPS spectrum, Si2p (HF treated, not treated))
- 09:47, 18 October 2011 Kn talk contribs uploaded File:XPS instrument2.JPG (XPS instrument)
- 09:44, 18 October 2011 Kn talk contribs uploaded a new version of File:XPS instrument.JPG (XPS instrument)
- 09:42, 18 October 2011 Kn talk contribs uploaded File:XPS instrument.JPG (XPS instrument)
- 16:27, 17 October 2011 Kn talk contribs uploaded File:Overview spectra Labadvisor.JPG (Overview spectra XPS from a Si sample)
- 16:13, 17 October 2011 Kn talk contribs uploaded File:XPS technique.JPG (XPS)
- 16:02, 17 October 2011 Kn talk contribs uploaded File:Si spectra Labadvisor.JPG (XPS Si spectrum)
- 15:54, 17 October 2011 Kn talk contribs uploaded File:Si spectra Labadvisor.pdf (XPS spectra of SiO)
- 14:43, 15 September 2011 Kn talk contribs uploaded File:Cryofox maskine.JPG (Picture of the PVD co-sputter/evaporation or cryofox machine.)
- 10:55, 15 September 2011 Kn talk contribs uploaded File:Stochiometry 20110510.JPG (Atomic % Ni and Cr in a NiCr wafer depsotited with settings described on the page about NiCr alloy.)
- 17:25, 17 February 2010 Kn talk contribs uploaded File:SiN cantilever dried CPD nr7.jpg (For CPD page: SiN cantilever dryed in Critical Point Dryer. Picture from Tom Larsen, Nanoprobes.)
- 17:21, 17 February 2010 Kn talk contribs uploaded File:SiN cantilever dried CPD.jpg (For CPD page: SiN cantilever dried in Critcal point dryer. Picture from Tom Larsen, Nanoprobes.)
- 17:06, 17 February 2010 Kn talk contribs uploaded File:SiN dried air.jpg (For CPD page: SiN cantilever dryed in air. Picture from Tom Larsen, Nanoprobes.)
- 16:50, 17 February 2010 Kn talk contribs uploaded File:SiN cantilever dryed air.ppt (For CPD page: SiN cantilever dryed in air. Picture from Tom Larsen, Nanoprobes.)
- 15:25, 17 February 2010 Kn talk contribs uploaded File:CPD.JPG (Picture of the Critical Point Dryer.)
- 14:07, 29 May 2009 Kn talk contribs moved page Fff to Critical Point Dryer
- 17:09, 16 December 2008 Kn talk contribs uploaded File:Au word rate5 .jpg (AFM picture of Au surface deposited in Wordentec. Dep. rate 5 Å/s. Size 2.5x2.5 my, the surface is uniform. )
- 16:34, 16 December 2008 Kn talk contribs uploaded File:AFMpict Cu Alc rate10.jpg (AFM picture of a Cu layer deposited in Alcatel. Dep. rate 10 Å/s.)
- 16:32, 16 December 2008 Kn talk contribs uploaded File:AFMpict Cu Alc 10Å S.jpg (AFM picture of a Cu layer deposited in Alcatel. Dep. rate 10 Å/s.)
- 14:52, 8 September 2008 Kn talk contribs uploaded File:W 21 thermal al.jpg (AFM picture of Al deposited with thermal deposition in Wordentec.)
- 09:18, 8 September 2008 Kn talk contribs uploaded File:Tiw 150W 0 001 nr2.jpg (AFM picture of sputter deposited TiW. Settings used: 150 W, 0.001mbar, 5 min)
- 11:12, 13 August 2008 Kn talk contribs uploaded File:Cr 404W 001mbar.jpg (AFM picture of sputter deposited Cr layer. Settings used: 405 W, 0.001 mbar.)
- 10:14, 13 August 2008 Kn talk contribs uploaded File:Cr 405W 004mbar.jpg (AFM picture of Cr layer sputter deposited in Wordentec. Settings: 405W, 0.004mbar)
- 08:37, 13 August 2008 Kn talk contribs uploaded File:E beam Cr 10Angs s.jpeg (AFM picture of Cr layerdeposited with e-beam evaporation in Wordentec. Deposition rate 10 Å/s.)
- 16:34, 12 August 2008 Kn talk contribs uploaded File:E beam Cr 10Angs s.ppt
- 16:34, 12 August 2008 Kn talk contribs uploaded a new version of File:E beam Cr 10Å s.ppt (AFM picture of e-beam deposited Cr layer, deposited with Wordentec. Rate 1 nm/s.)
- 16:29, 12 August 2008 Kn talk contribs uploaded File:E beam Cr 10Å s.ppt (AFM picture of Cr layer deposited with E-beam evaporation in Wordentec. Deposition rate 10 Å/s.)
- 11:43, 12 August 2008 Kn talk contribs uploaded File:Cr 150W 001mbar.jpg (AFM picture of sputter deposited Cr layer. 150W and 0.001 mbar used.)
- 11:33, 12 August 2008 Kn talk contribs uploaded File:Cr 150W 001mbar.JPG (AFM picture of sputtered Cr layer 150 W and 0.001 mbar used )