Jump to content

Specific Process Knowledge/Etch/Wet Aluminium Etch: Difference between revisions

Kabi (talk | contribs)
Kabi (talk | contribs)
Line 42: Line 42:
|PES 77-19-04  
|PES 77-19-04  
77 vol% Phosphoric acid 85%  
77 vol% Phosphoric acid 85%  
</br>
 
19 vol% Acetic acid 100%
19 vol% Acetic acid 100%
</br>
 
4 vol% Nitrid acid 70%  
4 vol% Nitrid acid 70%  
|-
|-