Specific Process Knowledge/Etch/Wet Aluminium Etch: Difference between revisions
Appearance
| Line 41: | Line 41: | ||
|H<sub>2</sub>O:H<sub>3</sub>PO<sub>4</sub> 1:2 | |H<sub>2</sub>O:H<sub>3</sub>PO<sub>4</sub> 1:2 | ||
|PES 77-19-04 | |PES 77-19-04 | ||
77 vol% Phosphorsyre 85% | |||
19 vol% Eddikesyre 100% | |||
4 vol% Salpetersyre 70% | |||
|- | |- | ||