At the anode metallic nickel is oxidized to nickel ions:
At the anode metallic nickel is oxidized to nickel ions:
   
   
Ni (s)  Ni2+ (aq) + 2 e-
Ni (s)  Ni<sup>2+</sup> (aq) + 2 e<sup>-</sup>
   
   
At the cathode (the sample surface), nickel ions from solution are reduced to metallic nickel:
At the cathode (the sample surface), nickel ions from solution are reduced to metallic nickel:
   
   
Ni2+ (aq) + 2 e-  Ni (s)
Ni<sup>2+</sup> (aq) + 2 e<sup>-</sup> Ni (s)
   
   
The minimal charge accepted by the software on the machine is 0.1 Ah (Ampere-hours). This corresponds to roughly 2 µm of nickel on a four inch wafer. You can abort a program prematurely to achieve even lower thicknesses, but this requires manual control of the machine.
The minimal charge accepted by the software on the machine is 0.1 Ah (Ampere-hours). This corresponds to roughly 2 µm of nickel on a four inch wafer. You can abort a program prematurely to achieve even lower thicknesses, but this requires manual control of the machine.