Specific Process Knowledge/Etch/Etching of Silicon Nitride: Difference between revisions
Appearance
| Line 181: | Line 181: | ||
*Typically 40-50 nm/min can be increased or decreased by using other recipe parameters. | *Typically 40-50 nm/min can be increased or decreased by using other recipe parameters. | ||
| | | | ||
*Process dependant. Tested once to ~60nm/min | |||
| | | | ||
*Process dependant. Has not been tested yet. | *Process dependant. Has not been tested yet. | ||