== Comparing silicon etch methodes at Danchip [[Image:section under construction.jpg|70px]]==
== Comparing silicon etch methodes at Danchip [[Image:section under construction.jpg|70px]]==


There are a broad varity of silicon etch methodes at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs.  
There are a broad varity of silicon nitride etch methods at Danchip. The methodes are compared here to make it easier for you to compare and choose the one that suits your needs.  


===Wet etches:===
===Wet etches:===