Specific Process Knowledge/Etch/Etching of Polymer: Difference between revisions
Appearance
No edit summary |
|||
| Line 7: | Line 7: | ||
<br clear="all" /> | <br clear="all" /> | ||
== | == Etching of Polymers == | ||
Stripping of polymers are often done by wet chemistry in a solvent that dissolves the given polymer. If wet chemistry cannot be used or a more controled etch of the polymer is needed a plasma system is used instead. Plasma ashers are design for removing polymers in primarily oxygen plasmas. It you need a more directional etch with a masking material RIE2 or ASE can be used. | Stripping of polymers are often done by wet chemistry in a solvent that dissolves the given polymer. If wet chemistry cannot be used or a more controled etch of the polymer is needed a plasma system is used instead. Plasma ashers are design for removing polymers in primarily oxygen plasmas. It you need a more directional etch with a masking material RIE2 or ASE can be used. | ||
Revision as of 09:53, 9 April 2013
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Etching of Polymers
Stripping of polymers are often done by wet chemistry in a solvent that dissolves the given polymer. If wet chemistry cannot be used or a more controled etch of the polymer is needed a plasma system is used instead. Plasma ashers are design for removing polymers in primarily oxygen plasmas. It you need a more directional etch with a masking material RIE2 or ASE can be used.
Comparison method 1 and method 2 for the process
| ASE | Plasma asher 1 | Plasma asher 2 | RIE2 | By wet etch
| |
|---|---|---|---|---|---|
| Generel description | Generel description - method 1 | Generel description - method 2 | Generel description - method 3 | Generel description - method 4 | Generel description - method 5 |
| Parameter 1 |
|
|
|
|
|
| Parameter 2 |
|
|
|
|
|
| Substrate size |
|
|
|
|
|
| Allowed materials |
|
|
|
|
|