'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Gold click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Gold click here]''' | ||
==Etching of Gold== | ==Etching of Gold== | ||
Revision as of 11:00, 8 April 2013
Feedback to this page: click here
Etching of Gold
Etching of Gold can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Gold Etch Methods
| Au wet etch 1 | Au wet etch 2 | IBE (Ionfab300+) | |
|---|---|---|---|
| Generel description | Wet etch of Au using Iodine based chemistry | Wet etch of Au using Aqua Regina | Sputtering of Au - pure physical etch |
| Etch rate range |
|
|
|
| Etch profile |
|
|
|
| Masking material |
|
|
|
| Substrate size |
|
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|