Etching of Gold can be done either by wet etch, dry etch or by sputtering with ions.
Etching of Gold can be done either by wet etch, dry etch or by sputtering with ions.
*[[Specific Process Knowledge/Etch/Wet Gold Etch|Etching of Gold by wet etch]]
*[[Specific Process Knowledge/Etch/Wet Gold Etch|Etching of Gold by wet etch]]
*[[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|Sputtering of Al]]
*[[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBE Au etch|Sputtering of Au]]
<br clear="all" />
<br clear="all" />