| '''Chemical solution''' | | '''Chemical solution''' | ||
| | |Chrome ETCH 18 | ||
|HNO<sub>3</sub>:H<sub>2</sub>O:cerisulphate - 90ml:1200ml:15g | |HNO<sub>3</sub>:H<sub>2</sub>O:cerisulphate - 90ml:1200ml:15g | ||
|- | |- | ||