Jump to content

Specific Process Knowledge/Etch/Wet Chromium Etch: Difference between revisions

BGE (talk | contribs)
Created page with "==Wet etching of Chromium== [[Image:fumehoodetch-chrom.jpg|300x300px|thumb|Fume hood: positioned in cleanroom 2. <br />Wet Etch of Chromium can take place in a beaker in this ..."
 
Kb (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:wetchemistry@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Wet_Chrominum_Etch click here]'''
==Wet etching of Chromium==
==Wet etching of Chromium==
[[Image:fumehoodetch-chrom.jpg|300x300px|thumb|Fume hood: positioned in cleanroom 2. <br />Wet Etch of Chromium can take place in a beaker in this fume hood]]
[[Image:fumehoodetch-chrom.jpg|300x300px|thumb|Fume hood: positioned in cleanroom 2. <br />Wet Etch of Chromium can take place in a beaker in this fume hood]]