*~?nm/min | *~?nm/min | ||
| | | | ||
*~ | *~14 nm/min (depending on features size and etch load) | ||
| | | | ||
*~30nm/min (not tested yet) | *~30nm/min (not tested yet) | ||
Revision as of 15:08, 12 March 2013
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Etching of Chromium
Etching of chromium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Aluminium Etch Metodes
| Cr wet etch 1 | Cr wet etch 2 | ICP metal | IBE (Ionfab300+) | |
|---|---|---|---|---|
| Generel description | Wet etch of Cr that you need to mix your self | Wet etch of Cr premixed | Dry plasma etch of Cr | Sputtering of Cr - pure physical etch |
| Etch rate range |
|
|
|
|
| Etch profile |
|
|
|
|
| Substrate size |
|
|
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
|
|
|
|