Etching of Aluminium
Etching of aluminium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Aluminium etch metodes
| Al wet etch 1 | Al wet etch 2 | Al etch by ICP metal | Al sputtering by IBE (Ionfab300+) | |
|---|---|---|---|---|
| Generel description | Wet etch of pure Al | Wet etch of Al + 1.5% Si | Dry plasma etch of Al | Sputtering of Al - pure physical etch |
| Etch rate range |
|
|
|
|
| Etch profile |
|
|
|
|
| Substrate size |
|
|
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
|
|
|
|