Specific Process Knowledge/Etch/Etching of Aluminium: Difference between revisions
Appearance
| Line 44: | Line 44: | ||
*~350 nm/min (depending on features size and etch load) | *~350 nm/min (depending on features size and etch load) | ||
| | | | ||
* | *~30nm/min (not tested yet) | ||
|- | |- | ||