*~60nm/min (Al+1.5% Si) | *~60nm/min (Al+1.5% Si) | ||
| | | | ||
* | *~350 nm/min (depending on features size and etch load) | ||
| | | | ||
* | * | ||
|- | |- | ||
Revision as of 13:00, 12 March 2013
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
Etching of Aluminium
Etching of aluminium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison methode 1 and methode 2 for the process
| Al wet etch 1 | Al wet etch 2 | Al etch by ICP metal | Al sputtering by IBE (Ionfab300+) | |
|---|---|---|---|---|
| Generel description | Wet etch of pure Al | Wet etch of Al + 1.5% Si | Dry plasma etch of Al | Sputtering of Al - pure physical etch |
| Etch rate range |
|
|
|
|
| Etch profile |
|
|
|
|
| Substrate size |
|
| ||
| Allowed materials |
|
|