*PECVD1 (standard):~147nm/min | *PECVD1 (standard):~147nm/min | ||
*TEOS:~265nm/min | *TEOS:~265nm/min | ||
*Stoichiometric Si3N4:~0.75nm/min (Morten Bo Mikkelsen, March 2013) | |||
*Stoichiometric Si3N4:~0.75nm/min(Morten Bo Mikkelsen, March 2013) | |||
| | | | ||
*Wet thermal oxide:~25nm/min | *Wet thermal oxide:~25nm/min | ||