===Thermal evaporation materials===
===Thermal evaporation materials===


We currently only have [[Specific Process Knowledge/Thin film deposition/Deposition of Aluminium|Aluminium]] and [[Specific Process Knowledge/Thin film deposition/Deposition of Silver|Silver]] available to deposit through thermal evaporation.
We currently have [[Specific Process Knowledge/Thin film deposition/Deposition of Aluminium|Aluminium]], [[Specific Process Knowledge/Thin film deposition/Deposition of Silver|Silver]] and '''Germanium''' available to deposit through thermal evaporation.


===Sputter materials===
===Sputter materials===