'''Feedback to this page''': '''[mailto:pvd@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/ | '''Feedback to this page''': '''[mailto:pvd@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Silver click here]''' | ||
<!-- Replace "http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin film deposition/Deposition of Aluminium" with the link to the Labadviser page--> | <!-- Replace "http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin film deposition/Deposition of Aluminium" with the link to the Labadviser page--> | ||
Revision as of 12:39, 1 March 2013
Feedback to this page: click here
Deposition of Silver
Silver can be deposited by e-beam evaporation, by sputtering and by thermal evaporation. In the chart below you can compare the different methods on the different deposition equipment.
| E-beam evaporation (Alcatel) | Thermal evaporation (Wordentec) | E-beam evaporation (PVD co-sputter/evaporation) | Sputter evaporation (PVD co-sputter/evaporation) | Sputter evaporation (Wordentec) | |
|---|---|---|---|---|---|
| Batch size |
|
|
|
|
|
| Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean | RF Ar clean | RF Ar clean |
| Layer thickness | 10Å to 1µm | 10Å to 0.5µm (0.5µm not on all wafers) | 10Å to 1000Å | 10Å to about 5000Å | 10Å to about 3000Å |
| Deposition rate | 2Å/s to 15Å/s | 1Å/s to 10 Å/s | About 1Å/s | Dependent on process parameters. | Depending on process paramterers (see logbook) |
Thermal deposition of Silver - Process settings for thermal deposition of Silver in Wordentec