Line 52: Line 52:
|1Å/s to 10 Å/s
|1Å/s to 10 Å/s
|About 1Å/s
|About 1Å/s
|Depending on process paramterers
|Dependent on [[/Sputter rates for Ag PVD co-sputter/evaporation|process parameters]].
|Depending on process paramterers (see logbook)
|Depending on process paramterers (see logbook)
|-
|-