Specific Process Knowledge/Etch/RIE (Reactive Ion Etch): Difference between revisions
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/RIE_(Reactive_Ion_Etch) click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/RIE_(Reactive_Ion_Etch) click here]''' | ||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Silicon_Nitride&action=submit click here]''' | |||
== Etching using the dry etch technique RIE (Reactive Ion Etch) == | == Etching using the dry etch technique RIE (Reactive Ion Etch) == | ||
| Line 10: | Line 12: | ||
'''The user manuals, quality control procedures and results, user APVs, technical information and contact information can be found in LabManager:''' | '''The user manuals, quality control procedures and results, user APVs, technical information and contact information can be found in LabManager:''' | ||
<!-- remember to remove the type of documents that are not present --> | |||
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=18 RIE1 info page in LabManager], | [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=18 RIE1 info page in LabManager], | ||
| Line 30: | Line 33: | ||
|style="background:WhiteSmoke; color:black"|<b>RIE2</b> | |style="background:WhiteSmoke; color:black"|<b>RIE2</b> | ||
|- | |- | ||
!style="background:silver; color:black;" align="center"|Purpose | !style="background:silver; color:black;" align="center" width="60"|Purpose | ||
|style="background:LightGrey; color:black"|Dry etch of | |style="background:LightGrey; color:black"|Dry etch of | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
| Line 125: | Line 128: | ||
|- | |- | ||
|} | |} | ||
Revision as of 14:18, 12 February 2013
Feedback to this page: click here
Feedback to this page: click here
Etching using the dry etch technique RIE (Reactive Ion Etch)


At Danchip we have three RIE's. Two (RIE1 and RIE2) for etching silicon based materials, resist and polymers (mainly RIE2) and one (III-V RIE) for etching III-V materials. Here only RIE1 and RIE2 will be described.
The hardware of RIE1 and RIE2 is very similar, but you cannot count on that identical recipes on RIE1 and RIE2 perform exactly the same. In addition to that the main difference between RIE1 and RIE2 is the cleanness of the two equipment. In rough terms RIE1 is the clean system and the RIE2 is the dirty system. This means that in RIE2 opposed to RIE1 it is allowed to have small amounts of metals exposed to the plasma.
The user manuals, quality control procedures and results, user APVs, technical information and contact information can be found in LabManager:
Process information
- Etch of silicon using RIE
- Etch of silicon oxide using RIE
- Etch of silicon nitride using RIE
- Etch of photo resist using RIE
| Equipment | RIE1 | RIE2 | |
|---|---|---|---|
| Purpose | Dry etch of |
|
|
| Performance | Etch rates |
|
|
| Anisotropy |
|
| |
| Process parameter range | Max pressure |
|
|
| Max R.F. power |
|
| |
| Gas flows |
|
| |
| Substrates | Batch size |
|
|
| Allowed materials |
|
| |