==A few words about the furnace==
==A few words about the furnace==
The furnace is a Tempress horisontal furnace. The process is a batch process meaning you can run a batch of 25 wafers at a time. The deposition takes place at temperatures of 800-850 degrees Celsius. The LPCVD nitride has a good step coverage and the film thickness is very uniform over the wafer. We have two standard LPCVD nitride processes: One for depositing stoichiometric nitride (Si<sub>3</sub>N<sub>4</sub>) and one for deposition low stress nitride (SNR).
The furnace is a Tempress horisontal furnace. The process is a batch process meaning you can run a batch of 25 wafers at a time. The deposition takes place at temperatures of 800-850 degrees Celsius. The LPCVD nitride has a good step coverage and the film thickness is very uniform over the wafer. We have two standard LPCVD nitride processes: One for depositing stoichiometric nitride (Si<sub>3</sub>N<sub>4</sub>) and one for deposition of low stress nitride (SNR).


{| border="1" cellspacing="0" cellpadding="3" align="center"
{| border="1" cellspacing="0" cellpadding="3" align="center"