! In the image the following parameters are shown:
! width="200px"| In the image the following parameters are shown:
* Top Width (TW)
* Top Width (TW)
* Depth (D)
* Depth (D)

Revision as of 21:47, 4 February 2013

Parameters

Solid shade
In the image the following parameters are shown:
  • Top Width (TW)
  • Depth (D)
  • Bottom Width (BW)
  • Mid Width (MW)

To speed up the characterisation post-SEM the parameter 'Pixel Size' (PS) is added to the SEM databar.

Depth